ISOPRENE RUBBER—INDUSTRY GRADE HAIRUBBER JHIR

Product Details    MSDS Download (0B) | TDS Download (0B)

Test Items

Unit

Brand and  Indicators

JHIR-90

JHIR-80

JHIR-70

JHIR-60

Appearance

/

Block solid

Mooney viscosity

/

   85-95

75-84

   65-74

   55-64

Viscosity  scattering in batch

/

8

8

8

8

Tensile strength at  23  

MPa

   ≥27

≥27

    ≥27

    ≥26

Elongation at  break

%

   ≥500

≥500

    ≥500

≥500

300% Set the  stretching stress

MPa

 measured

measured

  measured

measured

Ash

%

   ≤0.5

≤0.5

    ≤0.5

≤0.5

Drying loss

%

≤0.6

≤0.6

    ≤0.6

≤0.6


Application Field
  1. JHIRis synthetic rubber, no protein content,high content of cis-1:4,Low content of impurities,Itsmachining performance is similar to natural rubber.

  2. JHIRmainly used in tire ,conveyor belt ,tapes etc. replace natural rubber.