THERMOPLASTIC ELASTOMER SIS SERIES PRODUCTS

    HAI-SISTM  JH-SIS


    Specification

    TestItemsUnitGrade and Indicators
    JH-8151JH-8152JH-8153JH-8161JH-8291
    Styrenewt%15-1715-1715-1714-1628-30

    Diblock

    Content
    wt%-16-1819-2149-51-
    Melt Flow Rateg/10min8-128-1411-158-148-14
    HardnessShore A35-5530-4525-3526-3560-75
    Tensile StrengthMPa≥7≥7≥7≥4≥12
    Elongation at break%≥1000≥1000≥1000-≥800
    Solution ViscositymPa·s1300-17001000-1400600-1800700-1100300-500
    Ashwt%≤0.15≤0.15≤0.3≤0.15≤0.15
    VolatileMatterwt%≤0.7≤0.7≤1.0≤0.7≤0.7

    (1)TestConditions:200℃/5Kg.

    (2)TestConditions:25 wt% in Toluene; 25℃.